{"hasMore":true,"more":{"id":"tbaleAnchor_more","label":"\u66f4\u591a"}} {"hasMore":true,"more":{"id":"tbaleAnchor_more","label":"\u66f4\u591a"},"anchors":[{"id":"tbaleAnchor_applications","label":"\u5e94\u7528"},{"id":"tbaleAnchor_technical","label":"Technical Documents"},{"id":"tbaleAnchor_manual","label":"Manuals"}]} {"key":3506,"max":null,"filter":"Applications"} {"title":"\u5e94\u7528","columnTitle":"\u5e94\u7528","source":"product","key":3506,"filter_types":["applications","application_note","posters"],"config_list":[],"anchor":"tbaleAnchor_applications","filter":true} {"title":"Technical Documents","columnTitle":"Technical Documents","source":"product","key":3506,"filter_types":["technical","technical_reports","white_papers","primers"],"config_list":[],"anchor":"tbaleAnchor_technical","filter":true} {"title":"Manuals","columnTitle":"Manuals","source":"product","key":3506,"filter_types":["manuals"],"config_list":[],"anchor":"tbaleAnchor_manual","filter":true}
 

应用

无铅焊锡焊料中Ag与Cu的分布

对无铅焊锡焊料中大量含有Ag的区域进行面分析的数据。(加速电压:10kV;照射电流:20nA)
Ag的X射线像中颗粒形状与BSE像(COMPO)的颗粒形状一致。直径约0.1μm的Ag颗粒也清晰可辨(红色虚线圈出)。同时可确认Cu颗粒的存在(黄色虚线圈出)。

 

生物体组织中的金属元素

以下数据为EPMA捕捉到的肿瘤细胞中铂(Pt)元素图像,通过靶向给药将抗肿瘤药物卡铂(铂络合物)导入小鼠头颈部肿瘤组织中后进行分析检测。
卡铂通过与癌细胞内的遗传因子DNA链结合,阻碍DNA的分裂(复制)以杀灭癌细胞,利来国际最老品牌可以通过元素图像了解抗癌药物以何种形态进入癌细胞内。